Fire Performance of Connections in Laminated Veneer Lumber
The embedment strength of timber with respect to exposure temperature has not been widely studied. Some studies have suggested that the timber totally loses its embedment strength when the timber temperature reaches 300℃. This research concentrates on the embedment strength study of Laminated Veneer...
Main Author: | Chuo, Terence Chung Biau |
---|---|
Language: | en |
Published: |
University of Canterbury. Civil Engineering
2008
|
Subjects: | |
Online Access: | http://hdl.handle.net/10092/1131 |
Similar Items
-
Fire Resistance of Connections in Laminated Veneer Lumber (LVL)
by: Lau, Puong Hock
Published: (2008) -
Investigation of Single and Two Bolt Connections Perpendicular to Grain in Laminated Veneer Lumber
by: Patel, Monil Chintan
Published: (2014) -
Bolt Spacing and End Distance of Bolted Connection of Laminated Veneer Lumber (LVL) Sengon
by: Ali Awaludin, et al.
Published: (2017-03-01) -
Bolt Spacing and End Distance of Bolted Connection of Laminated Veneer Lumber (LVL) Sengon
by: Ali Awaludin, et al.
Published: (2017-03-01) -
Performance of Link-To-Stub Bolted Connection in Column-Tree Moment Resisting Frames under Fire Conditions
by: Mahmood Yahyai, et al.
Published: (2015-12-01)