Fire Performance of Connections in Laminated Veneer Lumber
The embedment strength of timber with respect to exposure temperature has not been widely studied. Some studies have suggested that the timber totally loses its embedment strength when the timber temperature reaches 300℃. This research concentrates on the embedment strength study of Laminated Veneer...
Main Author: | |
---|---|
Language: | en |
Published: |
University of Canterbury. Civil Engineering
2008
|
Subjects: | |
Online Access: | http://hdl.handle.net/10092/1131 |