High temperature corrosion during waste incineration : characterisation, causes and prevention of chlorine-induced corrosion

Waste-fired boilers suffer severely from corrosion of critical components such as superheater tubes. In this work the high temperature corrosion of candidate superheater alloys have been investigated by detailed laboratory studies and controlled field exposures in full-scale boilers. In a laboratory...