Varmduktilitet vid stränggjutning av duplexa rostfria stål

Abstract Hot ductility during continuous casting of duplex stainless steels In the continuous casting of the duplex stainless steel, longitudinal corner cracks in the first casted bloom of SAF 2507 have been discovered by Sandvik. SAF 2205 contains the same alloying substances as SAF 2507, but with...