Study of the leaching of goethite and hematite.
The direct dissolution of various samples of hematite and goethite in hydrochloric, sulphuric and perchloric acids using a particulate (-65, + 150 mesh) feed has been investigated. The reductive dissolution of hematite samples using acidified sulphur dioxide solutions was also investigated. Goethit...