Thermal Degradation Characteristics of Siloxane-Ether Urethane Copolymer
碩士 === 萬能科技大學 === 工程科技研究所 === 94 === Siloxane-ether urethane (PDMS/PTMG-PU) and siloxane-ether-imide urethane (PDMS/PTMG-PUIM) copolymers were synthesized in this study. The hard segments consisted of 4,4-diphenylmethane diisocyanate (MDI) and 1,4-butane diol (1,4-BD) or MDI and 3,3’,4,4’-diphenylsu...