碩士 === 國立海洋大學 === 材料工程研究所 === 90 === Hydrogen permeation rate and diffusivity in H900 specimen is lower than in SA specimen of 17-4 PH stainless steel. Hydrogen trapped in the interface between copper rich precipitates and matrix and caused brittle fracture in hydrogen environment. Hydrogen diffusio...
Main Authors: | , |
---|---|
Other Authors: | |
Format: | Others |
Language: | zh-TW |
Published: |
2002
|
Online Access: | http://ndltd.ncl.edu.tw/handle/57256111522248393964 |
id |
ndltd-TW-090NTOU0159006 |
---|---|
record_format |
oai_dc |
spelling |
ndltd-TW-090NTOU01590062015-10-13T12:47:22Z http://ndltd.ncl.edu.tw/handle/57256111522248393964 Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel 17-4PH析出硬化型不銹鋼氫脆之研究 B. L. Yu 余秉隆 碩士 國立海洋大學 材料工程研究所 90 Hydrogen permeation rate and diffusivity in H900 specimen is lower than in SA specimen of 17-4 PH stainless steel. Hydrogen trapped in the interface between copper rich precipitates and matrix and caused brittle fracture in hydrogen environment. Hydrogen diffusion path along grain and grain boundary in all specimens was observed by MPT. J. K. Wu 吳建國 2002 學位論文 ; thesis 88 zh-TW |
collection |
NDLTD |
language |
zh-TW |
format |
Others
|
sources |
NDLTD |
description |
碩士 === 國立海洋大學 === 材料工程研究所 === 90 === Hydrogen permeation rate and diffusivity in H900 specimen is lower than in SA specimen of 17-4 PH stainless steel. Hydrogen trapped in the interface between copper rich precipitates and matrix and caused brittle fracture in hydrogen environment. Hydrogen diffusion path along grain and grain boundary in all specimens was observed by MPT.
|
author2 |
J. K. Wu |
author_facet |
J. K. Wu B. L. Yu 余秉隆 |
author |
B. L. Yu 余秉隆 |
spellingShingle |
B. L. Yu 余秉隆 Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel |
author_sort |
B. L. Yu |
title |
Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel |
title_short |
Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel |
title_full |
Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel |
title_fullStr |
Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel |
title_full_unstemmed |
Hydrogen Embrittlement of 17-4 Precipitatipn Hardening Stainless Steel |
title_sort |
hydrogen embrittlement of 17-4 precipitatipn hardening stainless steel |
publishDate |
2002 |
url |
http://ndltd.ncl.edu.tw/handle/57256111522248393964 |
work_keys_str_mv |
AT blyu hydrogenembrittlementof174precipitatipnhardeningstainlesssteel AT yúbǐnglóng hydrogenembrittlementof174precipitatipnhardeningstainlesssteel AT blyu 174phxīchūyìnghuàxíngbùxiùgāngqīngcuìzhīyánjiū AT yúbǐnglóng 174phxīchūyìnghuàxíngbùxiùgāngqīngcuìzhīyánjiū |
_version_ |
1716866501311463424 |