The Manufacturing Process and Reliability Investigations of Si/Ta/TaCu/Cu/Ni-P/Sn-Pb Solder Bump
碩士 === 國立成功大學 === 材料科學及工程學系 === 89 === This research mainly investigated the solder bump structure of Si/Ta/TaCu/Cu/Ni-P/Sn-Pb, and integrated the best process parameter. First, we used the photolithography and alignment process to define the circle shape of which the diameter is 80 μm as a sputter...