Deuterium Retention in Polycrystalline Tungsten
Deuterium retention in two types of polycrystalline tungsten was studied as a function of ion fluence, irradiation temperature and ion energy. Fluence dependence: D retention at 300 K tends to saturate in both Rembar and Plansee PCW. At 500 K, D retention in the Plansee PCW increases with increasing...