An investigation on the surface austempering of ductile cast iron
This research presents surface austempering of ductile cast iron. Surface of pearlitic ductile cast iron samples were austenitised and heated to 810 and 850°C and held at these temperatures for 90 and 105 sec and then austempered at a temperature of 325°C for 60 and 90 min. The microstructure of sam...