Effect of sintering temperature on phase evolution of Al86Ni6Y4.5Co2La1.5 bulk amorphous composites synthesized via mechanical alloying and spark plasma sintering
Al86Ni6Y4.5Co2La1.5 amorphous powders were synthesized by mechanical alloying for 200 h. Subsequent consolidation was performed via spark plasma sintering in the temperature range of 250 °C to 500 °C at the pressure of 500 MPa. The role of viscous flow on densification was investigated by studying t...