Hard Copper with Good Electrical Conductivity Fabricated by Accumulative Roll-Bonding to Ultrahigh Strains
By modifying the accumulative roll-bonding (ARB) procedures, accumulative roll-bonding (ARB) processing up to 30 cycles (N) with a 50% thickness reduction per cycle (equivalent strain = 24) at room temperature was conducted on pure copper. The bonding condition, microhardness and electrical conducti...
Main Authors: | , , , , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2016-05-01
|
Series: | Metals |
Subjects: | |
Online Access: | http://www.mdpi.com/2075-4701/6/5/115 |