Preparation of gradient Ni-SDC anode by tape casting and co-sintering

Gradient Ni-SDC anode and anode-supported SDC electrolyte were produced by tape casting method with laminating and co-sintering process. The best co-sintering temperature of gradient Ni-SDC anode and SDC electrolyte was 1300°C for 3 h. The open porosity of gradient Ni-SDC anode sintered at 1300o...

Full description

Bibliographic Details
Main Authors: Li X.B., Wang H.Y., Gu H.X., Wang J., Zhang W.J., Wang T.G.
Format: Article
Language:English
Published: International Institute for the Science of Sintering, Beograd 2010-01-01
Series:Science of Sintering
Subjects:
Online Access:http://www.doiserbia.nb.rs/img/doi/0350-820X/2010/0350-820X1002153L.pdf