UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION

In this investigation feasibility of Beech slabs in particleboards production were prepared at three different contents resin of 9, 10, and 11 percent, press temperatures of 165°C and 175°C and hardener contents of 1.5 and 2.5 percent.Based on the DIN-68763 standard physical and mechanical propertie...

Full description

Bibliographic Details
Main Authors: Amir Nourbakhsh, Abdolrahman Hosseinzadeh, Kazem Doosthosseini, Abolfazl Kargarfard, Mazyar Radkyan
Format: Article
Language:fas
Published: Regional Information Center for Science and Technology (RICeST) 2005-05-01
Series:تحقیقات علوم چوب و کاغذ ایران
Subjects:
Online Access:http://ijwpr.areeo.ac.ir/article_117578_1d3f8c3270b49399ce92998c0b3fdceb.pdf
id doaj-f03bb689807d4c34a00e565c79578456
record_format Article
spelling doaj-f03bb689807d4c34a00e565c795784562020-11-25T02:12:55ZfasRegional Information Center for Science and Technology (RICeST) تحقیقات علوم چوب و کاغذ ایران1735-09132383-112X2005-05-0120شماره 111113210.22092/ijwpr.2005.117578117578UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTIONAmir Nourbakhsh0Abdolrahman Hosseinzadeh1Kazem Doosthosseini2Abolfazl Kargarfard3Mazyar Radkyan4Wood and forest products division, Research Institute of Forests and Rangelands, Agricultural Research Education and Extension Organization (AREEO), Tehran, IranWood and forest products division, Research Institute of Forests and Rangelands, Agricultural ResearWood and paper science and technology department, of natural Resources faculty, university of Tehran. IRANWood and Forest Products Science Research Division, Research Institute of Forests and Rangelands, Tehran, Iran,Islamic Azad University, Karaj, IranIn this investigation feasibility of Beech slabs in particleboards production were prepared at three different contents resin of 9, 10, and 11 percent, press temperatures of 165°C and 175°C and hardener contents of 1.5 and 2.5 percent.Based on the DIN-68763 standard physical and mechanical properties including MOR, MOE, IB, and thickness swelling (after 2 and 24 immersion in water) were tested.According to the factorial experimental design at completely random test was analysis. The potential utilization of Beech slabs residues in particleboard production including: resin content (11%), press time (6 min.), press temp. (175°C), and hardener contents (2.5%) were found.http://ijwpr.areeo.ac.ir/article_117578_1d3f8c3270b49399ce92998c0b3fdceb.pdfPARTICLEBOARDSbeechSLABS RESIDUESPRESS TIMERESIN CONTENTPRESS TEMPERATUREHARDENER CONTENT
collection DOAJ
language fas
format Article
sources DOAJ
author Amir Nourbakhsh
Abdolrahman Hosseinzadeh
Kazem Doosthosseini
Abolfazl Kargarfard
Mazyar Radkyan
spellingShingle Amir Nourbakhsh
Abdolrahman Hosseinzadeh
Kazem Doosthosseini
Abolfazl Kargarfard
Mazyar Radkyan
UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
تحقیقات علوم چوب و کاغذ ایران
PARTICLEBOARDS
beech
SLABS RESIDUES
PRESS TIME
RESIN CONTENT
PRESS TEMPERATURE
HARDENER CONTENT
author_facet Amir Nourbakhsh
Abdolrahman Hosseinzadeh
Kazem Doosthosseini
Abolfazl Kargarfard
Mazyar Radkyan
author_sort Amir Nourbakhsh
title UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
title_short UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
title_full UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
title_fullStr UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
title_full_unstemmed UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
title_sort utilization of beech slabs residues in particleboards production
publisher Regional Information Center for Science and Technology (RICeST)
series تحقیقات علوم چوب و کاغذ ایران
issn 1735-0913
2383-112X
publishDate 2005-05-01
description In this investigation feasibility of Beech slabs in particleboards production were prepared at three different contents resin of 9, 10, and 11 percent, press temperatures of 165°C and 175°C and hardener contents of 1.5 and 2.5 percent.Based on the DIN-68763 standard physical and mechanical properties including MOR, MOE, IB, and thickness swelling (after 2 and 24 immersion in water) were tested.According to the factorial experimental design at completely random test was analysis. The potential utilization of Beech slabs residues in particleboard production including: resin content (11%), press time (6 min.), press temp. (175°C), and hardener contents (2.5%) were found.
topic PARTICLEBOARDS
beech
SLABS RESIDUES
PRESS TIME
RESIN CONTENT
PRESS TEMPERATURE
HARDENER CONTENT
url http://ijwpr.areeo.ac.ir/article_117578_1d3f8c3270b49399ce92998c0b3fdceb.pdf
work_keys_str_mv AT amirnourbakhsh utilizationofbeechslabsresiduesinparticleboardsproduction
AT abdolrahmanhosseinzadeh utilizationofbeechslabsresiduesinparticleboardsproduction
AT kazemdoosthosseini utilizationofbeechslabsresiduesinparticleboardsproduction
AT abolfazlkargarfard utilizationofbeechslabsresiduesinparticleboardsproduction
AT mazyarradkyan utilizationofbeechslabsresiduesinparticleboardsproduction
_version_ 1724907427081486336