UTILIZATION OF BEECH SLABS RESIDUES IN PARTICLEBOARDS PRODUCTION
In this investigation feasibility of Beech slabs in particleboards production were prepared at three different contents resin of 9, 10, and 11 percent, press temperatures of 165°C and 175°C and hardener contents of 1.5 and 2.5 percent.Based on the DIN-68763 standard physical and mechanical propertie...