Influencia del envejecimiento higrotérmico en el comportamiento a fractura de compuestos de matriz termoplástica
Aging was carried out by introducing the materials into a climatic chamber under appropriate conditions of temperature, humidity and time. The materials are made of two types of weaving (2/2 Twill, 8H Satin) glass fibre, and (8H Satin) carbon fibre. The matrix was polyetherimide(PEI). In order to ch...