Enduring and Stable Surface Dielectric Barrier Discharge (SDBD) Plasma Using Fluorinated Multi-Layered Polyimide

In this work, multi-layered polyimide (PI) films were surface fluorinated at 328 K and 0.05 MPa using F2/N2 mixture with 20% F2 by volume, for a fluorination time of 0, 30 and 60 min, respectively. Then, they were subjected to discharge plasma as barrier dielectrics of surface dielectric barrier dis...