Hot Deformation Behavior and Microstructure Evolution of Cu–Ni–Co–Si Alloys

The Cu-1.7Ni-1.4Co-0.65Si (wt%) alloy is hot compressed by a Gleeble-1500D machine under a temperature range of 760 to 970 °C and a strain rate range of 0.01 to 10 s<sup>−1</sup>. The flow stress increases with the extension of strain rate and decreases with the rising of deformation tem...