Electrophoretic deposition and thermal treatment of boehmite coatings on titanium
An aqueous boehmite sol was prepared by the peptization of Al(OH)3. The electrophoretic deposition of boehmite coatings on titanium from the aqueous sol was performed at a constant voltage (from 1.0 to 10 V) and for a constant deposition time (from 10 to 30 min). Increasing the applied voltage and d...
Main Authors: | Đošić Marija S., Mišković-Stanković Vesna B., Srdić Vladimir V. |
---|---|
Format: | Article |
Language: | English |
Published: |
Serbian Chemical Society
2007-01-01
|
Series: | Journal of the Serbian Chemical Society |
Subjects: | |
Online Access: | http://www.doiserbia.nb.rs/img/doi/0352-5139/2007/0352-51390703275D.pdf |
Similar Items
-
Electrophoretic deposition and thermal treatment of boehmite coatings on titanium
by: MARIJA S. DJOSIC, et al.
Published: (2007-03-01) -
Electrophoretic deposition of alumina and boehmite coatings on metal surfaces
by: Vesna Miskovic-Stankovic
Published: (2012-12-01) -
Reactive hot pressing of boehmite
by: Bradbeer, Ross Stanley
Published: (2011) -
Approche multi-échelle de l'agrégation dans le procédé de précipitation de boehmite.
by: Kirchner, Sara
Published: (2015) -
Creep of compacts of colloidal boehmite (A100H) during dehydroxylation
by: St-Jacques, Robert Gustave
Published: (2011)