Electrophoretic deposition and thermal treatment of boehmite coatings on titanium

An aqueous boehmite sol was prepared by the peptization of Al(OH)3. The electrophoretic deposition of boehmite coatings on titanium from the aqueous sol was performed at a constant voltage (from 1.0 to 10 V) and for a constant deposition time (from 10 to 30 min). Increasing the applied voltage and d...

Full description

Bibliographic Details
Main Authors: Đošić Marija S., Mišković-Stanković Vesna B., Srdić Vladimir V.
Format: Article
Language:English
Published: Serbian Chemical Society 2007-01-01
Series:Journal of the Serbian Chemical Society
Subjects:
Online Access:http://www.doiserbia.nb.rs/img/doi/0352-5139/2007/0352-51390703275D.pdf