Oxidation - Nitridation of Ni-Cr-Al alloys
A series of alloys containing 24-36 wt pct Cr and 13.5 - 25.0 wt pct Al was reacted with air at 1100°C for 260 h. The products of isothermal reaction were scales of a-Al2O3 plus small amounts of Cr2O3. These grew according to parabolic kinetics, interrupted by episodic weight losses caused by partia...