Relation between microstructure, properties and spark plasma sintering (SPS) parameters of pure ultrafine WC powder

A combined experimental/numerical methodology is developed to fully consolidate pure ultrafine WC powder under a current-control mode. Three applied currents, 1900, 2100 and 2700 A, and a constant pressure of 20 MPa were employed as process conditions. The developed spark plasma sintering (SPS) fini...

Full description

Bibliographic Details
Main Author: Giovanni Maizza et al
Format: Article
Language:English
Published: Taylor & Francis Group 2007-01-01
Series:Science and Technology of Advanced Materials
Online Access:http://www.iop.org/EJ/abstract/1468-6996/8/7-8/A14