Microstructure, Texture Evolution and Magnetic Properties of Fe-6.5 wt. % Si and Fe-6.5 wt. % Si-0.5 wt. % Cu Alloys during Rolling and Annealing Treatment
Sheets of Fe-6.5 wt. % Si and Fe-6.5 wt. % Si-0.5 wt. % Cu with the thickness of 0.3 mm have been produced by hot and warm rolling. The microstructure, texture evolution and magnetic properties of the two alloys were investigated. It was found that the addition of 0.5 wt. % Cu promoted the formation...