Permanent Deformation and Stiffness Degradation of Open Hole Glass/PA6 UD Thermoplastic Composite in Tension and Compression
UD glass/PA6 coupons with an open hole are subjected to tensile and compressive loading. Three layups: [0/90]<sub>5s</sub>, [+45/−45]<sub>5s</sub> and [+45/0/−45/90]<sub>3s</sub> with a shape based on ASTM D5766 were tested. Both monotonic loading as well as loadi...