Study on the high-temperature corrosion behavior of superheater steels of biomass-fired boiler in molten alkali salts’ mixtures

Alkali sulfates and chlorides may result in rapid corrosion attack of the materials during the process of biomass-fired power generation. The 9-mm-thick 12Cr1MoV superheater tube in biomass-fired boiler was cut into samples by wire cutting. Hot corrosion behaviors of the materials in molten NaCl–50%...

Full description

Bibliographic Details
Main Authors: Jianjun He, Weizhou Xiong, Wei Zhang, Wei Li, Kailiang Long
Format: Article
Language:English
Published: SAGE Publishing 2016-11-01
Series:Advances in Mechanical Engineering
Online Access:https://doi.org/10.1177/1687814016678163