PART I. STUDY REGARDING THE OPTIMIZATION OF THE BIOSCOURING TREATMENT IN ULTRASOUND ON 60 % COTTON + 40 % COTTONISED FLAX MATERIALS

In the past years the commercial products for the bioscouring treatment were usually dedicated only for 100 % cotton or only for 100% lignocelluloses fabrics. The development of hemp/cotton or flax/cotton mixtures fabrics leds to the necessity of finding of the most apropiate products that could be...