The Low Strain Rate Response of As-Cast Ti-6Al-4V Alloy with an Initial Coarse Lamellar Structure

The microstructure and microtexture evolution of the as-cast Ti-6Al-4V alloy with an initial lamellar microstructure was investigated in the temperature range of 900–1050 °C and the low strain rate range of 10−3–10−1 s−1. In the ranges 900–950 °C and 10−3–10−2 s−1, globularization of the α lamellar...