Influence of mechanical activation on microstructure and crystal structure of sintered MgO-TiO2 system

Mixtures of MgO-TiO2 were mechanically activated using high-energy planetary ball mill during 5, 10, 20, 40, 80 and 120 minutes. Sintering process was preformed in air at 1100o-1400oC for 2h. The decrease in powder’s particle size was noticed as the time of mechanical activation increased and confir...