Creep crack growth behavior of P91 steel weldments
The steels operating at elevated temperatures are well known to be exposed to premature failure due to cracking caused by constant thermal stress, i. e. secondary creep process. Therefore, creep crack growth tests were carried out on compact tension specimens machined from P91 weld joint at 600°C to...
Main Authors: | Swei Mohamed, Sedmak Aleksandar S., Petrovski Blagoj, Golubović Zorana Z., Sedmak Simon A., Katinic Marko, Azzabi Khaled I. |
---|---|
Format: | Article |
Language: | English |
Published: |
VINCA Institute of Nuclear Sciences
2019-01-01
|
Series: | Thermal Science |
Subjects: | |
Online Access: | http://www.doiserbia.nb.rs/img/doi/0354-9836/2019/0354-98361700240S.pdf |
Similar Items
-
Creep and creep crack growth behaviors for base, weld, and heat affected zone in a grade 91 weldment
by: Woo-Gon Kim, et al.
Published: (2021-02-01) -
The microstructure and creep ductility of type 316 stainless steel weldments
by: Finlan, G.
Published: (1987) -
Microstructure and properties degradation of P/T 91, 92 steels weldments in creep conditions
by: Falat L., et al.
Published: (2012-01-01) -
Characterization of the cyclic softening and remaining creep behaviour of P92 steel weldment
by: Wei Zhang, et al.
Published: (2021-11-01) -
On the Improvement of Creep-fatigue Behavior of Grade 91 Weldments
by: Payton, Tyler K.
Published: (2017)