Sodium diffusion in 4H-SiC
Sodium diffusion has been studied in p-type 4H-SiC. Heat treatments have been performed from 1200 °C to 1800 °C for 1 min to 4 h. Secondary ion mass spectrometry has been used to measure the sodium distribution. We show that sodium has a considerable mobility at 1200 °C in p-type 4H-SiC. On the othe...
Main Authors: | M. K. Linnarsson, A. Hallén |
---|---|
Format: | Article |
Language: | English |
Published: |
AIP Publishing LLC
2014-09-01
|
Series: | APL Materials |
Online Access: | http://dx.doi.org/10.1063/1.4895040 |
Similar Items
-
Thermal conductivity/diffusivity of SiC-Mullite and SiC-SiC composites
by: Russell, Laura M.
Published: (2014) -
Diffusion of silver in 6H-SiC
by: Hlatshwayo, Thulani Thokozani
Published: (2013) -
Surface Recombination Investigation in Thin 4H-SiC Layers
by: Karolis GULBINAS, et al.
Published: (2011-07-01) -
Radiation Defects in Heterostructures 3C-SiC/4H-SiC
by: A.A. Lebedev, et al.
Published: (2019-02-01) -
Improvements in Realizing 4H-SiC Thermal Neutron Detectors
by: Issa F., et al.
Published: (2016-01-01)