PRODUCTION OF THE WROUGHT INGOTS OF HYPOEUTECTIC SILUMIN
It is shown that casting in crystallizer with flood-fluid power cooling system allows to produce the wrought ingots out of hypereutectic silumin without application of additional operations of thermoplastic deformation and annealing.