Contact strength of C-S-H cement phase
The object of the study was the cement phase C-S-H – X-ray amorphous calcium hydrosilicates, obtained by steaming at 80°C together limestone and silica at different molar ratios CaO/SiO2 = 0.5; 1.0; 1.5. The contact strength of the C-S-H phase with additions of portlandite, silica and alumina zols,...
Main Authors: | Ovcharenko Gennadiy, Ibe Ekaterina, Sandrasheva Aizhana, Viktorov Artem |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2019-01-01
|
Series: | E3S Web of Conferences |
Online Access: | https://www.e3s-conferences.org/articles/e3sconf/pdf/2019/23/e3sconf_form2018_02031.pdf |
Similar Items
-
Assessment of the influence of additives in concrete by the Raman spectroscopy method
by: Ovcharenko Gennadiy, et al.
Published: (2020-01-01) -
The effect of added high-iron slag on the frost resistance of cement compositions
by: Ovcharenko Gennadiy, et al.
Published: (2021-01-01) -
Strength and phase composition of autoclaved material: an approximation
by: Gennady Ovcharenko, et al.
Published: (2018-11-01) -
Durability of Novel C-S-H-based Nanocomposites and Secondary Hydrated Cement Phases
by: Khoshnazar, Rahil
Published: (2015) -
Phase composition and strength of cement stone with a complex additive
by: Shabanova Galina, et al.
Published: (2017-01-01)