Contact strength of C-S-H cement phase

The object of the study was the cement phase C-S-H – X-ray amorphous calcium hydrosilicates, obtained by steaming at 80°C together limestone and silica at different molar ratios CaO/SiO2 = 0.5; 1.0; 1.5. The contact strength of the C-S-H phase with additions of portlandite, silica and alumina zols,...