Effect of temperature and hydrogen concentration on the threshold stress intensity factor of radial delayed hydride cracking in fuel cladding
Three-point bending tests provide the ability to measure the propagation of axially oriented cracks in thin-walled fuel cladding in a radial outside-in direction. Via three-point bending, unirradiated Zircaloy-2 cladding containing 155 and 305 wppm hydrogen was mechanically loaded at different tempe...
Main Authors: | Bertsch, J. (Author), Colldeweih, A.W (Author) |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier B.V.
2022
|
Subjects: | |
Online Access: | View Fulltext in Publisher |
Similar Items
-
Bulk Hydrides and Delayed Hydride Cracking in Zirconium Alloys
by: TULK, ERIC
Published: (2012) -
Kinetic Model of Incipient Hydride Formation in Zr Clad under Dynamic Oxide Growth Conditions
by: Qianran Yu, et al.
Published: (2020-02-01) -
On the effect of temperature on the threshold stress intensity factor of delayed hydride cracking in light water reactor fuel cladding
by: Anna-Maria Alvarez Holston, et al.
Published: (2017-06-01) -
The effect of hydrogen and oxygen contents on hydride reorientations of zirconium alloy cladding tubes
by: Hyun-Jin Cha, et al.
Published: (2015-10-01) -
Hydride Rim Formation in E110 Zirconium Alloy during Gas-Phase Hydrogenation
by: Viktor Kudiiarov, et al.
Published: (2020-02-01)