Catalytic degradation of poly(methyl methacrylate) by zeolites and regeneration of used zeolites via ozonation
Catalytic degradation of PMMA was successfully performed at temperatures below 300°C. The use of zeolite catalyst could reduce reaction temperature in comparison with an ordinary thermal degradation process. It was found that the product distribution obtained from batch experiment depends on zeolite...
Main Author: | Khangkham, Supaporn |
---|---|
Format: | Others |
Published: |
2012
|
Online Access: | http://oatao.univ-toulouse.fr/9227/1/khangkham.pdf |
Similar Items
-
Catalytic degradation of poly(methyl methacrylate) by zeolites and regeneration of used zeolites via ozonation
by: Khangkham, Supaporn
Published: (2012) -
Catalytic Ozonation of Nitrobenzene by Manganese-Based Y Zeolites
by: Jingze Hu, et al.
Published: (2020-02-01) -
Catalytic studies on zeolites
by: Khan, M.
Published: (1986) -
Catalytic Studies on Zeolites
by: Gentry, S. J.
Published: (1973) -
Regeneration of catalytic modified zeolite to remove indoor bioaerosol and characteristics analysis
by: Chia-Hsi Tsai, et al.
Published: (2011)