Interaction between molten blister copper and 316L stainless steel
Blister copper is cast and usually processed further. At the Tsumeb Custom Smelter, Namibia, it is blown with nitrogen from mild steel lances, but these lances do not last long, causing down-time and reduced copper throughput. Additionally, the blister copper purity should be at least 98.5 wt% Cu, e...
Main Author: | Ilunga, Odilon Kasongo |
---|---|
Format: | Others |
Language: | en |
Published: |
2014
|
Online Access: | http://hdl.handle.net10539/13664 |
Similar Items
-
Corrosion Behavior of Eutectic Molten Salt solution on Stainless Steel 316L
by: Maksom, HF, et al.
Published: (2015) -
Electrochemical corrosion behavior of 316L stainless steel in molten fluorides with a temperature gradient
by: Yanli Wang, et al.
Published: (2019-12-01) -
Neutron irradiation of alloy N and 316L stainless steel in contact with a molten chloride salt
by: N. Dianne Bull Ezell, et al.
Published: (2021-03-01) -
Turning Research of Additive Laser Molten Stainless Steel 316L Obtained by 3D Printing
by: Grzegorz Struzikiewicz, et al.
Published: (2019-01-01) -
On the Interaction of Tritium with the Surfaces of Aluminum, Copper, Stainless Steel (type 316), and Gold
by: Sharpe, Matthew
Published: (2016)