Filamentary oxide formation on iron

The oxidation of iron in air or oxygen at temperatures between 300°C and 800°C is accompanied by the growth of filamentary crystals from the outer oxide surface. Below 470°C the predominant crystal habit is pointed platelets of approximately 10 μm thickness and 1-4 μm length, while above 470°C ribbo...