Designing Microstructure through Reverse Peritectoid Phase Transformation in Ni₃Mo Alloy
High-energy ball milling and powder metallurgy methods were used to produce a partially alloyed nickel and molybdenum of γ-Ni₃Mo composition (Ni-25at.%Mo). Milled powders were cold-compacted, sintered/solutionized at 1300°C for 100h sintering followed by quenching. Three transformation studies were...
Main Author: | Khalfallah, Ibrahim |
---|---|
Other Authors: | Materials Science and Engineering |
Format: | Others |
Language: | en_US |
Published: |
Virginia Tech
2017
|
Subjects: | |
Online Access: | http://hdl.handle.net/10919/78058 http://scholar.lib.vt.edu/theses/available/etd-12142016-092226/ |
Similar Items
-
Electrodeposition of Ni-Mo and Fe-Mo alloys from sulfate-citrate acid solutions
by: Sanches Luciana S., et al.
Published: (2003-01-01) -
Electrochemical deposition and characterization of Ni-Mo alloy powders
by: M.G. Pavlović, et al.
Published: (2007-12-01) -
Phase Transformation And Mechanical Properties Of Ti-12.1Mo-1Fe Alloy With Nano-Sized Precipitation
by: Lee D.-G., et al.
Published: (2015-06-01) -
Effects of Nb/Ti additions and heat treatment on the microstructure evolution and hardness of as-cast and directionally solidified NiAl–Cr(Mo) alloy
by: Zhao Shang, et al.
Published: (2021-01-01) -
Effect of Mo on the catalytic activity of Ni-based self-organizing catalysts for processing of dichloroethane into segmented carbon nanomaterials
by: Yury I. Bauman, et al.
Published: (2019-09-01)