Phase separation spinning of polypropylene fibers
Polypropylene fibers were spun from solutions of different polymer contents undergoing phase separation. The range of concentrations used was 25 to 60 wt. % polypropylene. The solvent used was naphthalene. After the naphthalene was extracted from the fibers using diethyl ether the fiber's prope...