Summary: | 碩士 === 義守大學 === 化學工程學系暨生物技術與化學工程研究所 === 105 === In this study, we will modify the glue formula to achieve the desired quality of products. And the glue is made from Acrylic resin that contains many compounds, including acetone and Isopropyl alcohol.
The main research object is acetone and Isopropyl alcohol, we will use the original formula (LC101T-3) to modify new formula (LC101T-8).
In the same conditions, we will analyze data of the two solvents to discover the rate of volatilization and coating defects interaction. And the temperature of each oven, will affect the rate of solvent evaporation and cause coating defects.
This research result, in the drying process of each oven, the data include solvent drying curve and number of defects,The LC101T-8 all better than LC101T-3.
However, The data of LC101T-8 explosive Limit is worse than LC101T-3, It may be the formulation adjustment has not achieved idealized.
|