Investigation into the Formation Mechanism of Defects on the Surface of Cu-Be Cooling Wheel by Cyclic Planar Flow Casting Process
碩士 === 義守大學 === 材料科學與工程學系 === 103 === Continuous casting of ribbon is accomplished by cyclic deposition of molten alloy onto a casting cooling wheel (e.g. C17200 Be-Cu alloy) and rapid quench. The cyclic molten metal contact and remove the solidified ribbon from the casting surface may result in man...
Main Authors: | Chih-Ping Li, 李治平 |
---|---|
Other Authors: | Huei-Sen Wang |
Format: | Others |
Language: | zh-TW |
Published: |
2015
|
Online Access: | http://ndltd.ncl.edu.tw/handle/dvc7ct |
Similar Items
-
Boiling phenomena of cooling water in the cooling wheel in the planar flow casting
by: Po-Sen Chen, et al.
Published: (2012) -
Effect of cooling circuit duration on formation of solidification shrinkage in A356 casting automative wheels
by: Lee, Rafael Jung Hoon
Published: (2008) -
Casting Defects in Transition Layer of Cu/Al Composite Castings Prepared Using Pouring Aluminum Method and Their Formation Mechanism
by: Chen Shuying, et al.
Published: (2019-02-01) -
Estimate influence of content carbon on the formation defects on the surface rail wheels at exploitation
by: L.I. Vakulenko, et al.
Published: (2012-08-01) -
Physical and computational models of free surface related defects in low-pressure die-cast aluminum alloy wheels
by: Duan, Jianglan