Wet Recovery Process for Tin Oxide Precipitates
碩士 === 明新科技大學 === 化學工程與材料科技系碩士班 === 101 === For the tin oxide precipitates from the treatment of spent tin stripping solution in the manufacture of printed circuit boards, the pure metallic tin can be recovered by using the wet recovery process. From the experimental study of high-temperature alkali...
Main Authors: | Jiang Yi-Yang, 江宜陽 |
---|---|
Other Authors: | Wu Jenn-Fang |
Format: | Others |
Language: | zh-TW |
Published: |
2013
|
Online Access: | http://ndltd.ncl.edu.tw/handle/12610874201408905660 |
Similar Items
-
Precipitation and stabilisation of colloidal tin (IV) oxide dispersions
by: Rebello, Alison
Published: (1999) -
Wet oxidation and etching processes applied on GaN optoelectronic devices
by: Ren-Hao Jiang, et al.
Published: (2013) -
Chemical precipitation and coatings of tin selenide
by: Z Zainal, et al.
Published: (2018-08-01) -
Chemical Precipitation and Coatings of Tin Selenide
by: Z Zainal, et al.
Published: (2017-10-01) -
Synthesis control and characterization of hydroxyapatite prepared by wet precipitation process
by: Maria Helena Santos, et al.
Published: (2004-12-01)