A Study of Hot Cracking Susceptibility during Welding on Incoloy 800H and 825 Superalloys.
碩士 === 國立中興大學 === 材料科學與工程學系所 === 100 === In this study, the hot cracking susceptibility of the Incoloy 800H and 825 nickel-base alloy substrate was discussed with filler and without filler. And later nickel alloy of filler 52 and 82 Tungsten inert gas shielded arc welding in the specimen. Observatio...
Main Authors: | Ching-Yi Pao, 包景毅 |
---|---|
Other Authors: | 吳威德 |
Format: | Others |
Language: | zh-TW |
Published: |
2012
|
Online Access: | http://ndltd.ncl.edu.tw/handle/33494026560692391696 |
Similar Items
-
Continuous Casting of Incoloy800H Superalloy Billet under an Alternating Electromagnetic Field
by: Fei Wang, et al.
Published: (2015-12-01) -
MODELLING AND CHARACTERIZATION OF LASER WELDED INCOLOY 800 HT JOINTS
by: Sathiya Paulraj, et al.
Published: (2016-06-01) -
Corrosion Damage Behavior of X65/Incoloy 825 Welded Bimetallic Composite Pipe in H2S Environment
by: Bingying Wang, et al.
Published: (2021-08-01) -
Weldability Evaluation in Autogenous Welds of Alloys 230, 800H, and 825
by: Suh, Sanghyun
Published: (2016) -
Weld development for Incoloy alloy 908, a low thermal expansion superalloy
by: Jang, Chang Heui
Published: (2005)