Effects of Rotary Swaging and Annealing on Mechanical Properties of AZ Series Magnesium Alloys
碩士 === 國立臺北科技大學 === 材料及資源工程系研究所 === 99 === AZ series magnesium alloys are rotary swaged and annealed at 100-400°C temperatures. The annealed microstructures and mechanical properties are observed. Mechanical properties of these alloys at 100-300°C temperatures are measured as well. The magnesium all...
Main Authors: | Chen-Yang Kao, 高振洋 |
---|---|
Other Authors: | J.K. Chen |
Format: | Others |
Language: | zh-TW |
Published: |
2011
|
Online Access: | http://ndltd.ncl.edu.tw/handle/32m2dg |
Similar Items
-
Effects of Neodymium and Rotary Swaging on Corrosion Behaviors of AZ71 Magnesium Alloys
by: Yu-Fen Lin, et al.
Published: (2014) -
Strain Hardening in an AZ31 Alloy Submitted to Rotary Swaging
by: Zuzanka Trojanová, et al.
Published: (2021-12-01) -
Achieving ultra-strong Magnesium–lithium alloys by low-strain rotary swaging
by: Yue Yang, et al.
Published: (2021-06-01) -
Structure, mechanical characteristics, biodegradation, and in vitro cytotoxicity of magnesium alloy ZX11 processed by rotary swaging
by: Natalia Martynenko, et al.
Published: (2020-12-01) -
Study on the effects of annealing on the microstructure and mechanical properties of AZ80 magnesium alloy
by: Li, Jun-Yi, et al.
Published: (2010)