Phase Transformations of the Ti- 5Al-1Sn -1Cr - 1Fe Alloy

碩士 === 國立屏東科技大學 === 機械工程系所 === 97 === During the continuous hot-rolling, the ultimate tensile strength, yielding strength and elongation of the Ti-5Al-1Sn-1Cr-1Fe alloy are in the range of 980~1060MPa, 860~1000MPa and 24-40%, respectively. The main purposes of the present studies are to investigate...