The Electrochemical properties of the main constituent phases of AZ91 magnesium alloys
碩士 === 國立成功大學 === 材料科學及工程學系碩博士班 === 97 === The electrochemical behavior of each constituent phase in AZ91D alloy was investigated. The Mg17Al12 (β) phase was prepared by melting Mg of 56 wt% and Al of 44 wt% in a crucible at 720˚C for 25 minutes. The mixed melt was cooled from 720˚C in a furnace and...
Main Authors: | Ya-Chu Chou, 周雅竹 |
---|---|
Other Authors: | Wen-Ta Tsai |
Format: | Others |
Language: | zh-TW |
Published: |
2009
|
Online Access: | http://ndltd.ncl.edu.tw/handle/55854464099431425012 |
Similar Items
-
A Comparative Electrochemical Study of AZ31 and AZ91 Magnesium Alloy
by: S. A. Salman, et al.
Published: (2010-01-01) -
Resistance of cast AZ91 magnesium alloy to electrochemical corrosion
by: Katarzyna Łyczkowska
Published: (2018-07-01) -
Comparison of Electrochemical Methods for the Evaluation of Cast AZ91 Magnesium Alloy
by: Jakub Tkacz, et al.
Published: (2016-11-01) -
Creep Properties of Magnesium Alloys AE44 and AZ91
by: Esho Faris, Nora
Published: (2019) -
Effect of Modification on Microstructure and Properties of AZ91 Magnesium Alloy
by: Andrzej Kiełbus, et al.
Published: (2020-06-01)