Preparation and Characteristics of the Glass Fiber/SiO2–Clay–TiO2/Epoxy Resin Composite Materials

碩士 === 逢甲大學 === 紡織工程所 === 97 === In this study, we first discuss the different layers of laminations via the resistance to compression test. It was determined that the best laminations consisted of 25 layers, with thermal conduction coefficient value of 0.069 W/m℃, compressive strength of 477.65 N/m...