The Study of Interface Characteristics Between the Opaque Porcelain and Ni-Cr-Mo-alloy
碩士 === 國立臺北科技大學 === 材料科學與工程研究所 === 96 === Porcelain was fired according to the manufacture''s instructions at 890℃, 975℃,and 1040℃ under vacuum condition. The bond strength testing was performed with a 3-point bending test. Specimens were examined of the metal-ceramic interface and micro-...
Main Authors: | Wen-Bin Zhuang, 莊文斌 |
---|---|
Other Authors: | 楊永欽 |
Format: | Others |
Language: | zh-TW |
Published: |
2008
|
Online Access: | http://ndltd.ncl.edu.tw/handle/5yrj82 |
Similar Items
-
Investigations of the Interface Properties between the Dental Porcelain and Ni-Cr-Mo Substrate
by: Qi-Ming Hong, et al.
Published: (2009) -
Microstructural Analysis of Dental Porcelain on Ni-Cr Alloy
by: Lin, S.H., et al.
Published: (1996) -
Effect of chemical composition on the corrosion resistance and metal/porcelain bonding characterization of Ni-Cr-Mo alloys
by: Mau-Chin Lin, et al.
Published: (2001) -
Effect of addition of recast materials on characteristics of Ni-Cr-Mo alloys
by: Walczak Mariusz, et al.
Published: (2019-06-01) -
Simulated Porcelain Firing of CO-CR Alloy
by: V. Dave, et al.
Published: (2019-12-01)