The Study of Interface Characteristics Between the Opaque Porcelain and Ni-Cr-Mo-alloy
碩士 === 國立臺北科技大學 === 材料科學與工程研究所 === 96 === Porcelain was fired according to the manufacture''s instructions at 890℃, 975℃,and 1040℃ under vacuum condition. The bond strength testing was performed with a 3-point bending test. Specimens were examined of the metal-ceramic interface and micro-...