Mechanical Alloyed Ti-based Amorphous Alloys with Significant Supercooled Liquid Region
碩士 === 國立海洋大學 === 材料工程研究所 === 88 === This study examined the amorphization behavior of Ti94-x-yCuxNiySi4B2 alloy powders synthesized by mechanical alloying technique. According to the results, after 5~7 hours of milling, the mechanically alloyed powders were amorphous at compositions with (x+y) equa...
Main Authors: | Nan-Fong Hsu, 許楠鋒 |
---|---|
Other Authors: | P. Y. Lee |
Format: | Others |
Language: | zh-TW |
Published: |
2000
|
Online Access: | http://ndltd.ncl.edu.tw/handle/38384370288494223728 |
Similar Items
-
The Study of Mechanical Alloyed Ni-Zr-Ti-Si Amorphous Alloys with Significant Supercooled Liquid Region
by: 方玉標
Published: (2001) -
Soft Magnetic Properties of Tin-added Fe-Based Amorphous Alloys with Large Supercooled Liquid Region
by: Chao Chih-Kang, et al.
Published: (2001) -
Ball Milling Parameters on the Supercooled Region of Ti64Ni30Si4B2 Amorphous Alloy
by: Chorng-Yong Lin, et al.
Published: (2000) -
The Structure of Amorphous and Deeply Supercooled Liquid Alumina
by: Caijuan Shi, et al.
Published: (2019-03-01) -
The Study of Mechanical Alloyed Zr-based Amorphous Alloy Powders with Extended Undercooled Liquid Region
by: Shih Wen Liu, et al.
Published: (2000)